Determination of the rate of corrosion of the main structural material of the grids of capillary phase separators

Oleksandr Minai

Abstract


The subject of this study is the corrosion processes that occur in the fuel tanks of spacecraft with a long service life, the engines of which operate on chemically aggressive fuel components (FC): nitrogen tetroxide (NT) and asymmetric dimethylhydrazine (NDMH). The goal is to determine the reduction of wire diameters and the increase of cell sizes of capillary phase separator grids (PSG) because of the corrosion effect of the main structural material of the 12X18H10T stainless steel grid. Task: establishing the presence, type, and rate of corrosion of the main structural material of the PSG nets. The methods used are as follows: to determine the presence of corrosion by studying the composition of substances found on the surface of the grids – X- ray fluorescence, X- ray structural, atomic absorption, potentiometric, turbodimetric, infrared spectroscopy, and chromato-mass spectrometry; to determine the type of corrosion-metallographic studies of mesh samples; to determine the rate of corrosion-measuring the geometric dimensions of mesh samples. The following results were obtained. The metal cations detected on the surface of the mesh samples correspond to the elements that make up the alloy of aluminum and steel - the main structural materials of the fuel tanks of launch vehicles; 12Х18Н10Т steel is not susceptible to local types of corrosion (pitting, intercrystalline, dot, contact, crevice, and stress corrosion cracking) in high-pressure and low-pressure tanks; the presence of a continuous (uniform) corrosion effect on the surface of the grid wires was established; dependences of changes in the main geometric parameters of the grids (wire diameters and cell sizes) over time were obtained, according to which the limits of the corrosion rates of stainless steel grade 12X18N10T in the liquid phase of NT and NDMG and in the gas phase were established; and coefficients of the maximum corrosion rate were calculated. Conclusions. The scientific novelty of the obtained results is as follows: for the first time, the presence, type, and rate of corrosion of the main structural material of the PSG grids because of their long-term operation (14...31 years) in the liquid phase of AT and NDMH and in the gas phase were determined using cross-methods.

Keywords


launch vehicle; microgravity; capillary phase separator; mesh phase separator; capillary retention capacity; fuel tanks; microstructure; corrosion; liquid rocket engine; reusable space systems; non-destructive testing; infrared spectroscopy; rocket fuels

References


Bagrov, V. V., Kurpatenkov, A. V., Polyaev, V. M. et al. Kapillyarnye sistemy otbora zhidkosti iz bakov kosmicheskih letatelnyh apparatov [Capillary liquid extraction systems from the tanks of space aircraft]. Moscow, UNPC "ENERGOMASH" Publ., 1997. 328 p. (in Russian).

Shevchenko, B. A. Raschetnyj i jeksperimental'nyj metod razrabotki sredstv zabora komponentov topliva iz bakov letatel'nyh apparatov s zhidkostnym raketnym dvigatelem [Estimated and experimental method for the development of means for collecting fuel components from tanks of aircraft with a liquid rocket engine]. dis. kand. teh. nauk. Dnepropetrovsk, KB «Juzhnoe» Publ., 1990. 209 p. (in Russian).

Chelomey, V. N., Polukhin, D. A., Mirkin, N. N. et al. Pnevmogidravlicheskie sistemy dvigatelnykh ustanovok s zhidkostnymi raketnymi dvigatelyami [Pneumohidraulic systems of propulsion systems with liquid rocket engines]. Moscow, Mashinostroenie Publ., 1978. 240 p. (in Russian).

Minai, O. M. Eksperymentalne vyznachennia zminy kapiliarnoi utrymnoi zdatnosti sitchastykh rozdiliuvachiv faz [Experimental determination of changes in capillary holding capacity of mash phase separators]. Aviacijno-kosmicna tehnika i tehnologia – Aerospace technic and technology, 2023, no. 6 (192), pp. 55-65. DOI: 10.32620/aktt.2023.6.07. (in Ukraine).

Minai, O., Ivanov, O., & Siedykh, I. Influence of long-term stay elements of capillary intake devices in liquid propellant components on their parameters. Aerospace Research in Bulgaria, 2020, vol. 32, pp. 175-192. DOI: 10.3897/arb.v32.e15.

Minai, O. M. Zmina kapiliarnoi utrymnoi zdatnisti zasobiv zabezpechennia sutsilnosti palyva v naslidok yikh tryvaloho terminu ekspluatatsii [Change in the capillary retention capacity of means of ensuring fuel integrity as a result of their long service life]. Visnyk DNU. Seriia: raketno-kosmichna tekhnika, zb. nauk. pry. – Herald of DNU. Series: rocket and space technology, coll of science avenue, 2023, vol. XXXI, pp. 58-73. DOI: 10.15421/452306. (in Ukraine).

Minai, O. M. Prediction of performance of mesh phase separators in GEO satellite capillary intake devices. 74th International Astronautical Congress . Baku , Azerbaijan , 02 – 06 October 2023, – Technical Presentation and Conference Paper IAC – 23, A2, 4, 4х76632. 10 p.

Minai, O. M. Vplyv na kapiliarnu utrymnu zdatnist sitchastykh rozdilnykiv faz yikh tryvaloho perebuvannia u komponentakh raketnoho palyva [Effect on the capillary retention capacity of mesh phase separators of their long stay in rocket fuel components]. Liudyna I kosmos: zb. tez. XXV Mizhnarod. molodizh. nauk.-prakt. konf. – Man and space: collection. theses XXV International youth science and practice conference, Dnipro, 2023, pp. 122-123. (in Ukraine).

Otchot ob opytno-rjystruktorskoj rabote «Analiz zapravok-slivov na vysokokipyshih komponentah topliva (Amil, Geptil)» [Report on experimental design work " Analysis experience of filling stations with plums on high-boiling fuel components (Amyl, Heptyl)"]. St. Petersburg, FGUP "RNC" Prikladnaya himiya" Publ., 2005. 46 p. (in Russian).

Hartwig, J., Johnson, W., Bamberger, H., Meyer, M., Wendell, J., Mullins, J., Robinson, R. C., & Arnett, L. NASA Glenn Research Center Creek Road Cryogenic Complex: Testing between 2005 – 2019. Cryogenics, 2020, vol. 106, pp. 1-12.

Sitka tkana z rvadratnymy oseredkamy mikronnykh rozmiriv. Tekhnichni umovy: 14-4-507-99 [Mesh woven with square cells of micron size. Technical conditions: TC 14-4-507-99]. Otrymuvach oryhinalu VAT “ Soniachnohirskyi zavod metalevykh sitok LEPSE” – Holder of the original of OJSC " Sonyachnohirsky Plant of Metal Meshes LEPSE" Publ., 1999. 2 p. (in Ukraine).

Minai, O. M. Shvydkist koroziinykh protsesiv ta yikh vplyv na zminu strukturnykh I heometrychnykh parametriv sitchastykh rozdiliuvachiv faz [The rate of corrosion processes and their influence on the change of structural and geometric parameters of mesh phase separators]. Kosmichni gorizonti: zb. tez. 3-i nauk.-prakt. inter.-konf. Vipusk №2 – Space horizons: collection. theses 3rd science and practice internet conference, Edition №2, Dnipro, 2023, pp. 36-40. (in Ukraine).